VY KARBONA ER70S-3 Metaly Fameno ho an'ny Fanesorana Arc Miaro amin'ny Gaz
Tariby MIG azo ampiasaina amin'ny asa rehetra ny ER70S3, izay mety amin'ny fampiasana vy karbônina maro. Tariby tsy misy oksidana vita amin'ny silikônina sy manganese izy io, ka mahatonga azy ho tsara indrindra amin'ny fanamboarana ankapobeny. Mila entona miaro ity vokatra ity.
Fampiasana mahazatra: fanamboarana ankapobeny, fanaka metaly, takelaka metaly, fanamboarana vy haingon-trano, fitaovana fambolena
| Kilasy AWS: ER70S3 | Fanamarinana: AWS A5.18/A5.18M:2005 |
| Firaka: ER70S3 | ASME SFA A5.18 |
| Toerana fanaovana welding: F, V, OH, H | Amin'izao fotoana izao: MIG-DCEP TIG-DCEN |
| Tanjaky ny fihenjanana, kpsi: | 70 |
| Tanjaky ny vokatra, kpsi: | 58 |
| Fanalavana amin'ny 2"%: | 22 |
Simia Tariby Mahazatra araka ny AWS A5.18 (ny sanda tokana no ambony indrindra)
| C | Mn | Si | P | S | Ni | Cr | Mo | V | Cu | |||
| 0.06-0.15 | 0.90-1.40 | 0.45-0.75 | 0.025 | 0.035 | 0.15 | 0.15 | 0.15 | 0.03 | 0.50 | |||
| Masontsivana mahazatra amin'ny fanendasana | ||||||||||||
| savaivony | DINGANA | Volta | Amps | Gaz miaro | ||||||||
| in | (mm) | |||||||||||
| .035 | (0.9) | GMAW | 28-32 | 165-200 | Famindrana famafazana 98% Argon + 2% Oksizenina na 75% Argon + 25% CO2 | |||||||
| .045 | (1.2) | GMAW | 30-34 | 180-220 | Famindrana famafazana 98% Argon + 2% Oksizenina na 75% Argon + 25% CO2 | |||||||
| 1/16 | (1.6) | GMAW | 30-34 | 230-260 | Famindrana famafazana 98% Argon + 2% Oksizenina na 75% Argon + 25% CO2 | |||||||
| .035 | (0.9) | GMAW | 22-25 | 100-140 | Famindrana herinaratra fohy 100% CO2 na 75% Argon +25% CO2 | |||||||
| .045 | (1.2) | GMAW | 23-26 | 120-150 | Famindrana herinaratra fohy 100% CO2 na 75% Argon +25% CO | |||||||
| 1/16 | (1.6) | GMAW | 23-26 | 160-200 | Famindrana herinaratra fohy 100% CO2 na 75% Argon +25% CO | |||||||
| 1/16 | (1.6) | GTAW | 12-15 | 100-125 | 100% Argon | |||||||
| 3/32 | (2.4) | GTAW | 15-20 | 125-175 | 100% Argon | |||||||
| 1/8 | (3.2) | GTAW | 15-20 | 175-250 | 100% Argon | |||||||